I am trying to look at an easy method of applying decals to an aircraft panel. There are lots of them. I did discuss this with Paul the other month but there seems to be no definitive way of doing this. I am currently looking at waterslide and the suggestion was applying this to the mould with a minimum tack before infusion. This could be prone to misalignment in the process. Using. Vinyl stencils seems a problem as the letters need to be small and precise alignment and then will require a silkscreen print to fill the vinyl stencils after removing. My thoughts are would it be better to create the panel, apply waterslide decals and then use an XCR resin coat to seal them forever in resin. Anyone experience of this and any advice would be appreciated.