Mold from ABS plastic part


Author
Message
Dan22h
Dan22h
Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)
Group: Forum Members
Posts: 15, Visits: 197
I have an abs plastic wheel arch liner for my car that I would like to take a mold from. I've read online that styrene based resins react with the ABS, is there any way around this such as suitable release agents? The part is not visible so surface finish isn't an issue.
Hanaldo
Hanaldo
Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
PVA release agent mate. Or packing tape. 
Fasta
Fasta
Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K


Are you sure it's ABS ?

The majority of modern plastic car bumper system fascias are made of thermoplastic olefins (TPOs), polycarbonates, polyesters, polypropylene, polyurethanes, polyamides, or blends of these with, for instance, glass fibers, for strength and structural rigidity.




Dan22h
Dan22h
Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)
Group: Forum Members
Posts: 15, Visits: 197
It's an inner wheel arch liner for a lotus exige, there's a paper sticker on the back with recycling logo ♻ >ABS<

Looks like this


Edited 9 Years Ago by Dan22h
Fasta
Fasta
Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)Supreme Being (4.6K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Do your own small test on the back of the part.

Some wax, some PVA and just a tiny bit of your preferred tooling gelcoat to see if it reacts.




Dan22h
Dan22h
Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)Supreme Being (115 reputation)
Group: Forum Members
Posts: 15, Visits: 197
OK, thanks for the replies.
FLD
FLD
FLD
posted 9 Years Ago HOT
Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
They are abs.  I'd go with the pva. Dust a light coat on with a spay gun and let it dry. Keep applying dust coats until you have an even blue coat then put down a few full film coats letting it dry between each coat. I then do a single coat of wax and grp just falls off!