What you are finding is the weight of the bonnet no longer helps compress the latch spring and that area flexes a little so you have to give it a bit of extra force to latch shut. You can add localised reinforcement to help reduce flex.
Adding soric will certainly improve stiffness and strength of the bonnet, however with enough force, it will still deflect. As long as you dont deflect it too much, it should still bounce back to shape.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|