Talk Composites - The Forum for Advanced Composites
Home
»
Advanced Composites Forum
»
General Composites Discussion
Bonnet Soric Question
http://www.talkcomposites.com/Topic23204.aspx
By joochrs
-
4/26/2017 7:17:23 AM
HI all,
I've managed to infused a few bonnets with top skin lay-up of 200g + 600g CF, with a patch of 600g reinforcement in the middle close to the latch.
The resulting skins are rather flexible on a large featureless area of the bonnet.
I know adding Soric to the lay-up would help stiffen up the skin.
But because of the light weight, I find I have to put more of my body weight into the bonnet when closing.
This flexes and dents the bonnet in the process (bounces right back when I'm off it)
Can the 200g+2mm Soric+200g lay-up in the tutorial take somebody putting their weight into the bonnet?
I sort of imagine the 200g+2mm Soric+200g lay-up making the skin "crunchy"
Would the Soric lay-up get permanently damaged if it's somehow dented?
Thank you!
Richard
By joochrs
-
4/27/2017 3:29:40 AM
Thank you, Warren.
Guess infused Soric is more flexible than I've imagined.
I will try localized reinforcement vs. soric/coremat to see which fits the bill better.