I have used EC high Temp Epoxy with pigment as a paint for brake calipers -- they lasted less than a year before starting to peel off... this was on a bike, that was occasionally used as a trackday tool ..
(Had some EC High temp and pigment, and was too cheap to go buy the "caliper paint" available Whistling)

On a normal road car, i would expect that the high temp would last much longer, since they will see much less UV and not go above 180 degrees C for longer periods (unless your brake pads hang Tongue)

Give it a go, and post pictures .. w00t

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Interloper393
Interloper393
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 90, Visits: 634
After looking at those I want to do it even more lol
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I would suggest those brake calipers don't see much use ^

One of my main concerns would be the difference in CTE between the carbon and the metal, as this would very likely cause the carbon to delaminate, at least in some areas. 
fibernoob
fibernoob
Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)
Group: Forum Members
Posts: 34, Visits: 134
Hi.

Besides the issues mentioned above with the actual laminate,  I  think you should also take into consideration that calipers need to dissipate the heat and cool down pretty fast.

Although it seems to have been done for show car purposes,   Check out this link : Audi RS 6 Carbon Fiber Trimmed Brake Calipers from Carbon Works Berlin
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I've not heard of skinned brake calipers before but doesn't mean it couldn't be done.  Biggest areas of concern are going to be temperature and long term durability.  I would suspect you would be looking at a high temperature resin in the vast majority oc cases.  You would be best to measure the actual temperature achieved to be on the safe side.

Long term durability might be an issue with constant temperature cycles, some nasty materials in brake pad dust, dust and debris from the road (wet and dry) etc.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Interloper393
Interloper393
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 90, Visits: 634
Hi guys,  I'm looking to skin a set of brake calipers for a guy,  has anyone done it?  If so what resins best to use?  I'm guessing I'd need to pop them in the oven to cure them at a high temp? 
Cheers
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search