Hi guys, I'm looking to skin a set of brake calipers for a guy, has anyone done it? If so what resins best to use? I'm guessing I'd need to pop them in the oven to cure them at a high temp?
Cheers
By Dravis
-
3/17/2017 10:35:53 AM
I have used EC high Temp Epoxy with pigment as a paint for brake calipers -- they lasted less than a year before starting to peel off... this was on a bike, that was occasionally used as a trackday tool ..
(Had some EC High temp and pigment, and was too cheap to go buy the "caliper paint" available
)
On a normal road car, i would expect that the high temp would last much longer, since they will see much less UV and not go above 180 degrees C for longer periods (unless your brake pads hang
)
Give it a go, and post pictures ..