Group: Forum Members
Posts: 5,
Visits: 42
|
Hi Warren,
Thanks for your quick reply,
Temperature wise, Probably 15-18 deg to start with, now I have the heating cranked up to 20-25 during the day but I have to turn it off at night (don't want to burn my shed down).
Mixing wise I'm pretty sure I got it right, the left overs in the pot has gone off like a rock.
Its Strange, it has "gone off" but its still greasy and a bit tacky on the surfice if I try and do anything to it.
I guess I will have to give it some more time and see how it goes.
I will let you know how it goes,
Drew.
|