newbie


Author
Message
jpongallo1
jpongallo1
Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)
Group: Forum Members
Posts: 6, Visits: 10
I'm new and just getting into carbon fiber work. I did my first mold and ended up with little success. My carbon fiber ended up gluing to my mold. This time i put 4 heavy coats of pva release agent to try and avoid this. What I really want to find out is making split moulds. Many of the parts i want to produce carbon fiber copies of have plastic parts on the back. Was thinking of 3d printing these and gluing them on or a split mold of some sort. any advice is welcomed.
Reply
jpongallo1
jpongallo1
Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)Forum Member (30 reputation)
Group: Forum Members
Posts: 6, Visits: 10
Not sure what the issue is? Did i press the carbon fiber down to hard?


http://www.talkcomposites.com/Uploads/Images/7d926d19-6bd2-46a5-b7ea-c580.jpg
Edited 8 Years Ago by jpongallo1
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search