Sticking parts in your mould is a common early mistake so in a way its good to have got that out the way now! Good application of release agents is vital to releasing your parts. It's good you learned that lesson now on a small part rather than a much bigger expensive part!
3D printing and bonding on the reverse fixings is a good way to finish the panels. The reverse fixings are a common issue for many when laminating and need to be considered on a case by case basis. Some people will take a cast of the fixings, then bond them in place, others will fabricate a new fixing from scratch. You can even bond in "big head" fasteners which will give you threaded studs/captive nuts etc which can help with refitting the panel.