The technique for skinning on a worktop would be exactly the same as any other item, albeit keeping the weave pattern straight is more important as it can be seen.
My main concern is temperature resistance. Hot oils, pans etc will mark even a post cured epoxy so it could well be vulnerable to damage if you are not careful.