Hi all,



I've got a few questions regarding the 'new' product 'XenCast Flexible Polyurethane Rubber' advertised on your website.

Basically I'm making a couple of moulds with the intention of casting 'Vac-Cast Epoxy Resin' into them,  what I need to end up with are two perfectly reproduced tooling plugs for vacuum forming my final parts into ABS plastic.



The following image will hopefully explain in greater detail my procedure.  I've recently used a product from 'Smooth-On' called 'OOMOO 30',  but had a disastrous result.  I must admit,  as good as it seems to be I just hate working with it.  Here's what my original mould box looks like with my plug secured in the base,  I then poured the silicon rubber into the mould box .........  it was an awful lot of work,  trying to mix what was a consistency of partly molten lava,  and the impossibility of pouring made the job needlessly difficult,  the result was a failed pour and a very badly formed mould  !  >>

 



Pouring the mix in a thin stream in a low corner was just impossible,  I almost had to resort to 'trowelling' it in ! >>

 



When I demoulded the following day,  it wasn't too bad,  but strictly speaking an appalling result.  Not something I would want to cast resin into that's for sure .........  I put it down to a good learning experience  >>





Because the silicon rubber wasn't 'fluid' enough,  full coverage of my plug wasn't achieved,  leaving large voids and air pockets  >>

 









So basically,  my question is,  would that 'XenCast flexible Polyurethane rubber'  be an alternative to OOMOO 30  ?

I've been looking at the 'XenCast PX30',  it seems to have the same characteristics as the OOMOO 30  ( both Shore A of 30 ),  how will it react to Vac-Cast Epoxy Resin being poured into it  ?







To further explain my situation my entire procedure is here >  Headlight mounting bracket moulds
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Hi Turk,

You will find most battery scales will have an auto shut off to protect battery life.  It is a bit frustrating if you need to leave the scales for a while mid measuring!

In terms of the silicone pulling from the wall of the box, I would not worry about it as in practice, the weight of the resin you pour into the mould will force it back against the box anyway so in practice there should be no problems.

I have a replacement vacuum gauge here which I will dispatch to you today so that should solve your problem.  Only thing to note is be careful how deep you pierce the bung to equalise pressure.  The max on the gauge is 4mm.  Some people have gone a fair bit deeper then hit the mechanism so be careful how deep you go.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
Warren (Staff) - 8 Years Ago
TURK - 8 Years Ago
Warren (Staff) - 8 Years Ago
TURK - 8 Years Ago
nc42 - 8 Years Ago
TURK - 8 Years Ago
Rich (Staff) - 8 Years Ago
TURK - 8 Years Ago
Rich (Staff) - 8 Years Ago
TURK - 8 Years Ago
Rich (Staff) - 8 Years Ago
TURK - 8 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
Warren (Staff) - 8 Years Ago
TURK - 8 Years Ago
TURK - 8 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
Warren (Staff) - 8 Years Ago
TURK - 8 Years Ago
Warren (Staff) - 8 Years Ago
Rich (Staff) - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
TURK - 8 Years Ago
TURK - 8 Years Ago
TURK - 8 Years Ago
TURK - 7 Years Ago
Hanaldo - 7 Years Ago
TURK - 7 Years Ago
Hanaldo - 7 Years Ago
TURK - 7 Years Ago
Hanaldo - 7 Years Ago
TURK - 7 Years Ago
Hanaldo - 7 Years Ago
TURK - 7 Years Ago
Hanaldo - 7 Years Ago
TURK - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search