Turk, if its only 5mm, I would shave down the chipboard ends of the box or use something thinner. It only needs to be strong enough to withstand the weight of the silicone once you pour it into the box. A Simple solution would be some 1mm steel or alloy as its thin and plenty strong enough and if you do it to both ends you should easily gain more than the 5mm you need.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|