Hi all,



I've got a few questions regarding the 'new' product 'XenCast Flexible Polyurethane Rubber' advertised on your website.

Basically I'm making a couple of moulds with the intention of casting 'Vac-Cast Epoxy Resin' into them,  what I need to end up with are two perfectly reproduced tooling plugs for vacuum forming my final parts into ABS plastic.



The following image will hopefully explain in greater detail my procedure.  I've recently used a product from 'Smooth-On' called 'OOMOO 30',  but had a disastrous result.  I must admit,  as good as it seems to be I just hate working with it.  Here's what my original mould box looks like with my plug secured in the base,  I then poured the silicon rubber into the mould box .........  it was an awful lot of work,  trying to mix what was a consistency of partly molten lava,  and the impossibility of pouring made the job needlessly difficult,  the result was a failed pour and a very badly formed mould  !  >>

 



Pouring the mix in a thin stream in a low corner was just impossible,  I almost had to resort to 'trowelling' it in ! >>

 



When I demoulded the following day,  it wasn't too bad,  but strictly speaking an appalling result.  Not something I would want to cast resin into that's for sure .........  I put it down to a good learning experience  >>





Because the silicon rubber wasn't 'fluid' enough,  full coverage of my plug wasn't achieved,  leaving large voids and air pockets  >>

 









So basically,  my question is,  would that 'XenCast flexible Polyurethane rubber'  be an alternative to OOMOO 30  ?

I've been looking at the 'XenCast PX30',  it seems to have the same characteristics as the OOMOO 30  ( both Shore A of 30 ),  how will it react to Vac-Cast Epoxy Resin being poured into it  ?







To further explain my situation my entire procedure is here >  Headlight mounting bracket moulds
Reply
TURK
TURK
Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)Supreme Being (1K reputation)
Group: Forum Members
Posts: 101, Visits: 662
Hi all,



This is all getting very confusing now,  to the point of being frustrating ..........

I've been looking at an alternative for the 'Smooth-On OOMOO 30' silicone rubber that I had a bad experience with.  I'm pretty sure I've found an alternative,  EC's 'CS25 Condensation Cure Silicone Rubber'.
Reading the DataSheet shows it would probably suite my needs,  but it shows that the viscosity is between 20,000 and 26,000 Cps.  'OOMOO 30' was rated at 4250 Cps ( like Maple Syrup basically ) .........  mine was more like trying to mix and pour tooth paste !

I've been searching around on the internet for a comparison,  just trying to imagine what it would be like to pour it ...........  unfortunately when you search for those terms,  20,000 Cps,  the results compares it to 'Silicone Rubber' !   Crying    ya,  I know !



So,  any ideas guys  ?  I am really stumped here ..........  all I want to do is to pour some silicon rubber in a mould    Sad











TURK
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
Warren (Staff) - 8 Years Ago
TURK - 8 Years Ago
Warren (Staff) - 8 Years Ago
TURK - 8 Years Ago
nc42 - 8 Years Ago
TURK - 8 Years Ago
Rich (Staff) - 8 Years Ago
TURK - 8 Years Ago
Rich (Staff) - 8 Years Ago
TURK - 8 Years Ago
Rich (Staff) - 8 Years Ago
TURK - 8 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
Warren (Staff) - 8 Years Ago
TURK - 8 Years Ago
TURK - 8 Years Ago
TURK - 8 Years Ago
Hanaldo - 8 Years Ago
Warren (Staff) - 8 Years Ago
TURK - 8 Years Ago
Warren (Staff) - 8 Years Ago
Rich (Staff) - 8 Years Ago
Hanaldo - 8 Years Ago
TURK - 8 Years Ago
TURK - 8 Years Ago
TURK - 8 Years Ago
TURK - 8 Years Ago
TURK - 7 Years Ago
Hanaldo - 7 Years Ago
TURK - 7 Years Ago
Hanaldo - 7 Years Ago
TURK - 7 Years Ago
Hanaldo - 7 Years Ago
TURK - 7 Years Ago
Hanaldo - 7 Years Ago
TURK - 7 Years Ago
Hanaldo - 7 Years Ago
TURK - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search