Kevlar with prepreg carbon?


Author
Message
James66
James66
Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)
Group: Forum Members
Posts: 10, Visits: 99
Hi all

Needing to do some carbon secondary motorcycle engine covers
Intending on doing these in prepreg however as they are to protect the main engine covers when sliding down the track I need to add another material such as kevlar/diolen to help resist the abrasion against the tarmac

How is best to do it when combining with prepreg?
Cheers
Reply
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
You could use a pre preg film glue and a layer of dry kevlar with the main pre preg cook and it will all wet out with all being done in one shot.