Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Pre Pregs cutting and making templates question
Pre Pregs cutting and making templates question
Post Reply
Like
3
Pre Pregs cutting and making templates question
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TomDesign
TomDesign
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
Hello guys
im thinking to build owen and yo buy easycomposites pre pregs . question is where to buy material cutter and how to make perfect templates?
Thank u
Reply
Like
3
Replies
TomDesign
TomDesign
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
ok guys i do infusion molds how to get nice overlaping join i mean then? my mirrors mold if from 4 pieces if i connect them i gonna see not nice dark line joined how to avoid that?
Reply
Like
2
morepower
morepower
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 242,
Visits: 1.2K
TomDesign (19/10/2016)
ok guys i do infusion molds how to get nice overlaping join i mean then? my mirrors mold if from 4 pieces if i connect them i gonna see not nice dark line joined how to avoid that?
You will get some line on any join to be honest. Its a fact of life. It is best to either accept it or try and do something to use the line to your advantage. Like making a V or an obvious change in direction.
This is out of the mould and not trimmed yet. I have a large join for the whole side of the tank. I cannot match the weave of the top along its whole length so it looks odd at some point. So I change the direction of the weave to make it more attractive to look at. But I also have to V the top which is a one piece mould section too so it adds work but makes the whole think look more visually attractive.
Hanaldo you can now see what I mean about the filler cap neck too.. The mould is very thick there so it takes a long time to cool so I have to lift the mould a little to clear the main body then just let it cool to allow it to come up with out damaging that neck area of the mould. With a carbon mould it just slides up nicely hot or cold.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Pre Pregs cutting and making templates question
TomDesign
-
9 Years Ago
Just cut it with a sharp knife. The surface ply can be cut with shears, the backing ply can too but...
Hanaldo
-
9 Years Ago
hanaldo text me your viber we talk more
TomDesign
-
9 Years Ago
https://www.youtube.com/watch?v=5XHj_JiD0d0 what about this cutting pre-pregs?
TomDesign
-
9 Years Ago
That's just a hot-wire cutter. Cuts that film by melting it. Would make a lovely mess of your...
Hanaldo
-
9 Years Ago
As hanaldo says cutting prepreg is easy. Unless you have zeveraly thousand for a vac ply cutting...
scottracing
-
9 Years Ago
Without having something like a CNC cutter when I want really accurate cutting of shapes I make an...
Fasta
-
9 Years Ago
ok guys you saw video from easycomposites guy that work for serious places say that this mold...
TomDesign
-
9 Years Ago
Nothing wrong with the Unimould system provided it's used within its capacities. I don't use...
Hanaldo
-
9 Years Ago
The Uni-Mould system is very good for out of autoclave pre-preg work as long as you keep to the...
Warren (Staff)
-
9 Years Ago
Any wet lay glass mould will have some shrinkage when you make a pre-preg part. It will warm up and...
morepower
-
9 Years Ago
Yeh that's true, the expansion can be a problem. To be honest I haven't had any real issues yet,...
Hanaldo
-
9 Years Ago
[quote][b]Hanaldo (19/10/2016)[/b][hr]Yeh that's true, the expansion can be a problem. To be...
morepower
-
9 Years Ago
ok guys i do infusion molds how to get nice overlaping join i mean then? my mirrors mold if from 4...
TomDesign
-
9 Years Ago
[quote][b]TomDesign (19/10/2016)[/b][hr]ok guys i do infusion molds how to get nice overlaping join...
morepower
-
9 Years Ago
so how i can join in infusion connect nicely mirrors if they from 4 pieces?
TomDesign
-
9 Years Ago
With infusion, unless you're using 'Profinish' fabric that has the resin binder to help hold it...
MarkMK
-
9 Years Ago
any images how overlaping results getting?
TomDesign
-
9 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search