Hi all,




I've been doing a lot of wet lay recently and it can be a lot of effort per part to ensure a pinhole free finish. I am looking to start resin infusing and wondered if anyone has any experience with the following pump:




http://www.ebay.co.uk/itm/2-5CFM-1-4HP-Single-Stage-Vacuum-Pump-Air-Conditioning-Refrigeration-Vacuum-5Pa-/122085713861?hash=item1c6ce027c5:g:xWwAAOSwgZ1XsW4m




Reason I ask is because its cheap! Will it be up to the job? the parts I am making are smaller than a dinner plate.




Also, is it risky to infuse without a catch pot/vacuum chamber if I leave enough silicone hosing on the pump side?




Best Regards,




James



Reply
James91h
James91h
Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)Supreme Being (167 reputation)
Group: Forum Members
Posts: 20, Visits: 217
Thank you for the info Warren, much appreciated.