good morning all. 

I have done a few moulds since my intro and I have just finished a mould and found it needs repairs doing in a small area. What would be the best way to repair any holes and cracks?

Thanks for your time and help in advance. 
Reply
Chris Smith
Chris Smith
Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)Forum Guru (73 reputation)
Group: Forum Members
Posts: 11, Visits: 436
I am using tooling jel coat. That's what I thought but wanted to make sure first. Thanks