I bought a resin infusion kit last year and had a go at making a flat panel which came out reasonably well, but didn't have a perfect surface finish as I had a slight vacuum leak and it ended up a bit 'resin light' with some imperfections aligned with the fibres.

I have been away with work a lot so not done much since then but made another flat panel last week. This time with a soric core. The surface finish on this is much better but it is possible to see some cloudy streaks in the finish. How is the best way to minimise these in the future? 

My thoughts were; it could be due to using the easylease which I used last year as I believe it goes off with time when opened or perhaps I didn't buff out the easylease enough when applying layers. Incidentally. It didn't feel like the panel released as easily as previously, which may add weight to the first point.

What's the best approach to minimise this cloudiness? Try some new easylease?

Thanks.
Oli
Replies
OliilO
OliilO
Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)
Group: Forum Members
Posts: 9, Visits: 126
It's quite hard to photo, but easy to see. I'll try and get some decent ones later.

They are slightly cloudy marks that do look as if it's where I have moved a cloth over the plastic sheet (used as a flat surface) when applying release agent. Would that be indicative of over application of easylease?
OliilO
OliilO
Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)
Group: Forum Members
Posts: 9, Visits: 126
http://s1290.photobucket.com/user/oli_lewis/library/Mobile%20Uploads?sort=3&page=1

Photos of the sheet are above. The cloudiness is reasonably clear in them.

The surface finish is great other than the cloudiness (and a random fibre that got in there Angry )
Edited 9 Years Ago by OliilO
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search