Nicholas Hedworth
Nicholas Hedworth
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 9
So I'm just a 16 year old kid introduced into the world of composites just a few weeks a go and I have been hooked on how they work and their different properties. Recently I have come across different types of weave for carbon fiber instead of just the the regular weave. So what i would like to know is how, say, the triaxial or quadraxial weave differs from the regular weave and how I might be able to obtain some on a consumer level since there isnt much information about them that i could find on the internet to satisfy me.
Thanks
Nick
Tags
#CarbonNoob
Reply
Like
7
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Quad, tri and biaxials are simply four, three, and two layers of unidirectional fabric that are stitched together at varying orientations to give you strength in multiple directions. The benefit is that unidirectional fabrics have less crimp than woven fabrics, so they are stronger and can have a lower resin content. So you could have a biaxial fabric with 0/90 orientation, which is the same fibre orientation as a woven plain or twill fabric, but it will be stronger (weight for weight) than the woven.
They are commercially available, but less so than woven fabrics simply due to demand. I believe EC have a triaxial carbon that you can purchase in small quantities.
Reply
Like
7
Rich (Staff)
Rich (Staff)
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 167,
Visits: 4.6K
Hi Nick and Hanaldo,
We don't have any Triax at the moment; Biaxial is available though in 300g +/-45' Orientation.
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search