So I'm just a 16 year old kid introduced into the world of composites just a few weeks a go and I have been hooked on how they work and their different properties. Recently I have come across different types of weave for carbon fiber instead of just the the regular weave. So what i would like to know is how, say, the triaxial or quadraxial weave differs from the regular weave and how I might be able to obtain some on a consumer level since there isnt much information about them that i could find on the internet to satisfy me.
Thanks
Nick
By Rich (Staff)
-
9/1/2016 9:36:03 AM
Hi Nick and Hanaldo,
We don't have any Triax at the moment; Biaxial is available though in 300g +/-45' Orientation.