Good morning All from Gloucestershire

I am new to this forum but not new to composites as I had worked for over 10 years at a Motorsport manufactures composite shop ( prepeg only and rather large Autoclaves)

I have on the road a 3.5 litre Dax Rush Kit Car and have decided to dabble with some home made composites and start to upgrade some part on the car.

My first project is to remake its bonnet scope in carbon fibre, I have purchased a Uni-mould kit from easy composites which I intend to lay up the scoop mould over the bank holiday weekend.

I am starting on the cheap first and will see if I can wet lay up a carbon skin or two first (once the mould is finished) to see what sort of finish I can get as I don't have access to ovens for curing and before investing in vacuum pumps and resin infusion etc as funds are a little tight.




So I am looking forward to asking for advice and welcoming comments on how to produce some good carbon parts for my car.




Regards

Ian
Edited 9 Years Ago by Porkster0
Reply
Porkster0
Porkster0
Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)
Group: Forum Members
Posts: 14, Visits: 69
Hi All

Just a quick update have just made and broken out my first mould and must say am very happy with the results see photos test 1 & 3.

I was worried that it would stick & never come apart again loosing my original scoop but followed instructions / advice given me on here and came apart so easy with an excellent finish and shine for main component area, apart from flanges .

Only one little bridge / loss of gelcoat say about 60 to 70mm long on a edge (might try and fill) as shown in photo test 2

Thanks again for help

Regards

Ian
Attachments
test 1.jpg (694 views, 323.00 KB)
test3.jpg (669 views, 417.00 KB)
test2.jpg (651 views, 185.00 KB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search