Tight corners can always be difficult. You can cut the peel ply and mesh into strips to make it easier to move around. I would only ditch mesh in hard areas if you are confident the resin will flow there anyway.
If there is a lot of resin build up in the corners, then that indicates you may well have a bit of bridging in those areas. having the strips of peel and mesh means the two can move slightly when you pull the vacuum making it a bit easier to get into those tight corners.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|