By Chris172 - 8/7/2016 11:41:21 AM
Hi guys im new to resin infusion I've made carbon parts for an 1984 rwd Toyota Starlet head lamp surrounds and front grill an I seem to have a problem with pulling of the Peelply an infusion mesh more so in tight angles was wondering do I actually need to put mesh in tight angle corners because of resin build up thanks in advance if anyone can help. So my first attempt didn't go so well let's say I wasn't very happy but kinda knew it would be trial an error second time around there were pretty good few little things in them but good enough to use.
|
By Chris172 - 8/8/2016 10:14:53 AM
Cheers warren will try that next time an I posts some pics of how I get on
|
|