ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 32,
Visits: 100
Ive been looking into making a valve cover or skinning a valve cover as well making an exhaust tip. Can this be done with Carbon fiber? Im assuming the Fiber itself can handle the heat but
im worried about the epoxy. Are there any that can handle high engine temps? or exhaust temps (muffler tip temps)
Reply
Like
3
Reply
ArturK
ArturK
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 19,
Visits: 53
Please remember that you need:
A) Resin with high TG (as linked)
B) Curing at high temperature (>100 C)
in order to have a composite that will have temperature resistance more than 100 C .
Carbon fiber sheets and composites .
www.dexcraft.com
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Carbon Fiber for parts that get hot
dcfoster
-
9 Years Ago
There is a high temp resin available...
meir
-
9 Years Ago
Thanks for the info Meir :)
dcfoster
-
9 Years Ago
Please remember that you need: A) Resin with high TG (as linked) B) Curing at high temperature...
ArturK
-
9 Years Ago
Im making an exhaust end cap for my motorcycle. It is just a surround really so not actually...
Boozehawk
-
9 Years Ago
Hi Boozehawk, Loading into an oven at 100'C is definitely not recommended - Firstly, before...
Rich (Staff)
-
9 Years Ago
[quote][b]Richie (15/08/2016)[/b][hr]Hi Boozehawk, The High Temp Epoxy has a recommend cure...
Boozehawk
-
9 Years Ago
Potentially but you would be likely to find that the surface of the resin would deform slightly as...
Rich (Staff)
-
9 Years Ago
What materials have you used to make your mould? Is it a polyester gelcoat with polyester laminating...
Hanaldo
-
9 Years Ago
Im not wanting a gloss finish so the part would be getting a rub. down after demolding anyway. I...
Boozehawk
-
9 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search