Carbon Fiber for parts that get hot


Author
Message
dcfoster
dcfoster
Supreme Being (205 reputation)Supreme Being (205 reputation)Supreme Being (205 reputation)Supreme Being (205 reputation)Supreme Being (205 reputation)Supreme Being (205 reputation)Supreme Being (205 reputation)Supreme Being (205 reputation)Supreme Being (205 reputation)
Group: Forum Members
Posts: 32, Visits: 100
Ive been looking into making a valve cover or skinning a valve cover as well making an exhaust tip. Can this be done with Carbon fiber? Im assuming the Fiber itself can handle the heat but
im worried about the epoxy. Are there any that can handle high engine temps? or exhaust temps (muffler tip temps)