Using Airpad in Laminate
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
scottracing
scottracing
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
Hi All
I've used Airpad several times for tooling and curing applications using prepreg in the laminate to add a bit of strength, however I now have a component that needs some impact protection and durability for a sports application.
I have used Kraibon material for such an application as you can incorporate it into the laminate, but we dont have any material in stock so I was hoping to use airpad instead although im scared it might delam.
Has anyone used Airpad inside a laminate? If so did it work and how many plies of carbon did you have on the surface layer?
Cheers
Gaz
Reply
Like
2
Reply
f1rob
f1rob
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 237,
Visits: 4.8K
Not used it but cant you beg,borrow or steal some smac rubber, or one of the generic copies ?
should give you what your looking for and you know its going to stick like the perverbial to the carbon
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Using Airpad in Laminate
scottracing
-
9 Years Ago
Not used it but cant you beg,borrow or steal some smac rubber, or one of the generic copies ?...
f1rob
-
9 Years Ago
cheers rob, I will see if i can get some of that rubber material, ive been given some airpad and...
scottracing
-
9 Years Ago
just an update on this , I done a 6 ply layup with the airpad in after the 2nd ply of carbon. Cured...
scottracing
-
9 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search