scottracing
scottracing
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
Hi All
I've used Airpad several times for tooling and curing applications using prepreg in the laminate to add a bit of strength, however I now have a component that needs some impact protection and durability for a sports application.
I have used Kraibon material for such an application as you can incorporate it into the laminate, but we dont have any material in stock so I was hoping to use airpad instead although im scared it might delam.
Has anyone used Airpad inside a laminate? If so did it work and how many plies of carbon did you have on the surface layer?
Cheers
Gaz
Reply
Like
5
f1rob
f1rob
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 237,
Visits: 4.8K
Not used it but cant you beg,borrow or steal some smac rubber, or one of the generic copies ?
should give you what your looking for and you know its going to stick like the perverbial to the carbon
Reply
Like
5
scottracing
scottracing
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
cheers rob,
I will see if i can get some of that rubber material, ive been given some airpad and also a roll of SVPP called Tegris which i will try out in the laminate. Never used it before but it looks pretty good for intrusion and side impact protection.
Reply
Like
5
scottracing
scottracing
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
just an update on this , I done a 6 ply layup with the airpad in after the 2nd ply of carbon. Cured at 135°C with a dwell for 3 hours and the part had come out ok although the tooling block didnt fair as good
but i cant glue it back together.
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search