I have a question about my experience with Soric. I have done an infusion twice with 2mm Soric and both times have had "pattern printing" of the Soric onto the cosmetic finish of the completed component. The first time, we thought we may have had an issue with the in-mold gelcoat and it's ability to set, so we did a second infusion without the gelcoat, and still have Soric printing. I would really like to use this product, but with the surface not being the level I want or expect, I am concerned I'll have to do something different.
|