hello everyone. i was wondering if you guys from easy composites could exlplain more about this, i´ve being wondering
about the uses and aplication of diferent types of Core Materials
sorry if it is a stupid question :/
im really curious about this, specially for automotive parts development, which ones/how/where they should be used
Replies
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi Lisanty,

There are very many different types of core materials that you can use in a composite laminate ('sandwich' composites), we stock some of the more popular or easy to use core materials and so given the wide range available I'll only summerise the ones we stock.

The idea of all core materials is to increase the thickness of a panel without increasing its weight, cost or layup time (depending on the core material and the production priorities) as much as solid reinforcement would. Because in a panel under load it's really the innermost and outermost skins that do the majority of the work and because increasing the thickness of a panel increases its stiffness significantly, low density core materials can be very effective in creating stiff, light panels.

COREMAT
The simplest core material of all. Really only used in wet-layup of conventional GRP parts. Lower density than solid glass but still with quite a high resin uptake so more of a time and cost saver than a weight saver.

LANTOR SORIC
Like an infusion grade version of coremat but with a much more sophisticated honeycomb-like cell structure. Soric will act as an internal flow media for resin during infusion (meaning resin flows through it easily and in fact Soric can function as the only resin flow facilitator in an infusion project). Soric has a medium resin uptake meaning that there are lower density core materials out there but almost none that are as easy to use. No special processing is required, just lay the soft, flexible honeycomb-like mat into your laminate before infusion. We sell this is 2mm and 3mm.

CLOSED CELL PVC FOAM
Lower density than Soric, easy to work with foam core material. Closed cell foam has good compressive strength, bonds well to resin systems (particularly epoxy resin) and needs no special processing. Being a 'closed cell' material means that it have virtually zero resin uptake and so it remains a low density core even after infusion. Suitable for wet-lay, vacuum bagging, resin infusion and pre-preg (depending on processing temperature). For co-infusion, the core MUST be drilled to allow resin to flow from the top skin to the bottom skin. Alternatively, upper and lower skins can be made in advance and then bonded together around the core.

ALUMINIUM HONEYCOMB
The highest performance (in terms of mechanical strength vs. density) of all core materials but certainly the most complicated to work with. Generally, when working with aluminium honeycombs (or even other honeycomb materials), it is necessary to make the two skins separately first and then bond in the honeycomb using a liquid honeycomb bonding adhesive or an adhesive film (such as Hexel's Redux 609). Aluminium honeycomb has excellent shear strength and good compressive strength and used correctly will result in the highest performance (hence its widespread use in aerospace and F1). Aluminium honeycomb is not suitable for infusion (because the cells would simply fill with resin) and so, as with other laminating methods, it is necessary to make both skins separately first.

I hope this gives you a good insight into these different core materials and what they can do for you. For further information, take a look at the product pages for the respective products where you'll find mechanical and process data (such as resin uptake, density, compressive and shear strength) which would be helpful when making comparisons.

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Lisanty
Lisanty
Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)
Group: Forum Members
Posts: 3, Visits: 30
Matt! thank you soooo much for this information! i really appreciate the work that you guys have being doing.

once again cheers Smile
alebassa
alebassa
Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)Supreme Being (332 reputation)
Group: Forum Members
Posts: 48, Visits: 171
Matt (Staff) (04/07/2012)
Hi Lisanty,

There are very many different types of core materials that you can use in a composite laminate ('sandwich' composites), we stock some of the more popular or easy to use core materials and so given the wide range available I'll only summerise the ones we stock.

The idea of all core materials is to increase the thickness of a panel without increasing its weight, cost or layup time (depending on the core material and the production priorities) as much as solid reinforcement would. Because in a panel under load it's really the innermost and outermost skins that do the majority of the work and because increasing the thickness of a panel increases its stiffness significantly, low density core materials can be very effective in creating stiff, light panels.



Thank you Matt, I was just looking for this explanation!


Alessandro
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
Matt (Staff) (04/07/2012)
Hi Lisanty,

There are very many different types of core materials that you can use in a composite laminate ('sandwich' composites), we stock some of the more popular or easy to use core materials and so given the wide range available I'll only summerise the ones we stock.

The idea of all core materials is to increase the thickness of a panel without increasing its weight, cost or layup time (depending on the core material and the production priorities) as much as solid reinforcement would. Because in a panel under load it's really the innermost and outermost skins that do the majority of the work and because increasing the thickness of a panel increases its stiffness significantly, low density core materials can be very effective in creating stiff, light panels.

COREMAT
The simplest core material of all. Really only used in wet-layup of conventional GRP parts. Lower density than solid glass but still with quite a high resin uptake so more of a time and cost saver than a weight saver.

LANTOR SORIC
Like an infusion grade version of coremat but with a much more sophisticated honeycomb-like cell structure. Soric will act as an internal flow media for resin during infusion (meaning resin flows through it easily and in fact Soric can function as the only resin flow facilitator in an infusion project). Soric has a medium resin uptake meaning that there are lower density core materials out there but almost none that are as easy to use. No special processing is required, just lay the soft, flexible honeycomb-like mat into your laminate before infusion. We sell this is 2mm and 3mm.

Matt

Could you comment on nomex honeycomb please. 

Thanks

Fred

CLOSED CELL PVC FOAM
Lower density than Soric, easy to work with foam core material. Closed cell foam has good compressive strength, bonds well to resin systems (particularly epoxy resin) and needs no special processing. Being a 'closed cell' material means that it have virtually zero resin uptake and so it remains a low density core even after infusion. Suitable for wet-lay, vacuum bagging, resin infusion and pre-preg (depending on processing temperature). For co-infusion, the core MUST be drilled to allow resin to flow from the top skin to the bottom skin. Alternatively, upper and lower skins can be made in advance and then bonded together around the core.

ALUMINIUM HONEYCOMB
The highest performance (in terms of mechanical strength vs. density) of all core materials but certainly the most complicated to work with. Generally, when working with aluminium honeycombs (or even other honeycomb materials), it is necessary to make the two skins separately first and then bond in the honeycomb using a liquid honeycomb bonding adhesive or an adhesive film (such as Hexel's Redux 609). Aluminium honeycomb has excellent shear strength and good compressive strength and used correctly will result in the highest performance (hence its widespread use in aerospace and F1). Aluminium honeycomb is not suitable for infusion (because the cells would simply fill with resin) and so, as with other laminating methods, it is necessary to make both skins separately first.

I hope this gives you a good insight into these different core materials and what they can do for you. For further information, take a look at the product pages for the respective products where you'll find mechanical and process data (such as resin uptake, density, compressive and shear strength) which would be helpful when making comparisons.

Ian P
Ian P
Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)Junior Member (16 reputation)
Group: Forum Members
Posts: 2, Visits: 8
Thank you for a really good overview, from me too! Would be grateful for some slightly more specific advice if that's ok?

We're planning to build a carbon/kevlar/glass sumpguard for a rally car, the current design uses layers of carbon and glass with a kevlar skin on the underneath (for its wear/penetratin performance). The glass layers are essentially to add bulk in the middle and I was looking at your core materials as being a potentially more effective alternative.

The guard will be bolted up onto brackets on the car, obviously the crush strength of the core material at the mountings will be critical. I'm wary of using the aluminium honeycomb because it creates a hollow, so was thinking that something like Coremat would be suitable, am I on the right track? Will it sustain the compression loads associated with bolting up and (obviously) impacts?

Many thanks in anticipation
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Lisanty - 14 Years Ago
Matt (Staff) - 14 Years Ago
Lisanty - 14 Years Ago
alebassa - 13 Years Ago
fgayford - 13 Years Ago
Ian P - 12 Years Ago
MNM - 14 Years Ago
Matt (Staff) - 14 Years Ago
MNM - 14 Years Ago
Matt (Staff) - 13 Years Ago
MNM - 13 Years Ago
altaran - 13 Years Ago
Warren (Staff) - 13 Years Ago
altaran - 13 Years Ago
TheEngineer - 13 Years Ago
Farbin Kaiber - 13 Years Ago
Warren (Staff) - 13 Years Ago
     Thanks!
TheEngineer - 13 Years Ago
carbonfibreworks - 12 Years Ago
Ian P - 12 Years Ago
ajb100 - 12 Years Ago
brainfart - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search