Group: Forum Members
Posts: 58,
Visits: 401
|
Hi, on my car i have a carbon lip on the front bumper. This gets a beating and to fix it i sanded it down and applied ef80 flexible resin.
Now i must have done something wrong when mixing as im at day 3 now and it still hasnt cured, its just sticky when i put my finger on it and its sticks to my finger when i remove it.
So the question is what do i do, will it eventually cure? or how do i remove it and start over with the process? Sanding it now will definetly not work =)
|