By Ronny - 6/7/2016 10:04:18 AM

Hi, on my car i have a carbon lip on the front bumper.
This gets a beating and to fix it i sanded it down and applied ef80 flexible resin.

Now i must have done something wrong when mixing as im at day 3 now and it still hasnt cured, its just sticky when i put my finger on it and its sticks to my finger when i remove it.

So the question is what do i do, will it eventually cure? or how do i remove it and start over with the process?
Sanding it now will definetly not work =)
By Ronny - 6/7/2016 2:40:34 PM

Yes i noticed the high hardened ratio and i mixed 50g resin and 75g hardener +-3grams.
So i know frem earlier that this is very important to get 100% right, but that thought passed my mine after the resin had been applied Smile

So the damage is done, i just need to know how to mend it.