Like I say, a light dusting is fine, even if you're going to prepare it with Easy-Lease because effectively you'll be rubbing all the solvent based paint away; the time to worry is if you're using it as a complete coat for your pattern.
Matt Statham Easy Composites / Carbon Mods - Technical Sales
|