Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Like I say, a light dusting is fine, even if you're going to prepare it with Easy-Lease because effectively you'll be rubbing all the solvent based paint away; the time to worry is if you're using it as a complete coat for your pattern.

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
congellous
congellous
Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)
Group: Forum Members
Posts: 9, Visits: 71
Oh that's no use then as I am going to use easi lease and mould wax is there any alternative to expose the high and low spots when I'm flattening ?
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi,

If you're just using a very light dusting of a contrasting coloured paint as a means of identifying high and low spots as you flat then that should be OK however if you're talking about a full coating of rattle-can primer then I would be very nervous of that - rattle can paints wreak havock with release agents and so are best avoided where possible.

--Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
congellous
congellous
Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)Supreme Being (93 reputation)
Group: Forum Members
Posts: 9, Visits: 71
Hi all, I'm finishing my plug to a nice finish, can I spray with a primer from a can to expose any imperfections ?
or any suggestions to achieve the result 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search