By congellous - 7/2/2012 11:39:18 AM

Hi all, I'm finishing my plug to a nice finish, can I spray with a primer from a can to expose any imperfections ?
or any suggestions to achieve the result 
By Matt (Staff) - 7/2/2012 1:30:17 PM

Like I say, a light dusting is fine, even if you're going to prepare it with Easy-Lease because effectively you'll be rubbing all the solvent based paint away; the time to worry is if you're using it as a complete coat for your pattern.