Hey all,

Once again, have finally got a bit of time to upload some photos so thought I'd post some of the work I have been doing lately. Have got a few of 57 Chev builds that I've been doing work for, so will start with those.

Did the pattern work, mould and final parts for this radiator duct and inner guards:

https://scontent.fper1-1.fna.fbcdn.net/hphotos-xap1/v/t1.0-9/12310622_738911766240242_9110443415019921671_n.jpg?oh=cd7fde5c3eb81e70f6605b408adca2ba&oe=57775AD2


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xla1/v/t1.0-9/12347916_738911786240240_3721986100639564617_n.jpg?oh=d5d588f718af7b6fd6160219ab0b52fc&oe=577ECC85


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xla1/v/t1.0-9/12316508_738911802906905_8433533168459750719_n.jpg?oh=9eb13c7355911b399f68b5896d25d3e1&oe=57745B7F


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xal1/v/t1.0-9/12308280_738911826240236_2149852792654226814_n.jpg?oh=1ff72d6d6b2262c73ec7ce393665e82e&oe=577EBB26


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xtl1/v/t1.0-9/12299399_738911859573566_5905637213753825989_n.jpg?oh=9088d646a4ef0da01aab053b70f79dfe&oe=57776C08


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xal1/v/t1.0-9/12301566_738913199573432_2409998155294452604_n.jpg?oh=d2ad9d7f71bc0dbc92314760cf2c9430&oe=577352B0


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xfa1/v/t1.0-9/12342324_738913219573430_102750671480467473_n.jpg?oh=9f22ca0a909776ab9986b22d101ea45e&oe=577DAC37


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xaf1/v/t1.0-9/12310695_738913239573428_2150057675047925559_n.jpg?oh=c5f9fad917e9d994fb904b5f407c8842&oe=577F81D0


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xal1/v/t1.0-9/12342498_738913359573416_2725935529982062647_n.jpg?oh=14c7bfcb24fbf53bec17abefcd4a3594&oe=57BEC82D








https://scontent.fper1-1.fna.fbcdn.net/hphotos-xal1/v/t1.0-9/12341215_740232169441535_1343449809717540780_n.jpg?oh=89554b10956f0681bc8d442a8d779d7e&oe=57BEBCC3




https://scontent.fper1-1.fna.fbcdn.net/hphotos-xlp1/v/t1.0-9/12341423_740232149441537_7789396152532162957_n.jpg?oh=51b71a1e8cd6b187cc04e379edb7b0c4&oe=5781EEB0
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Also made this Alufibre dash binnacle amongst all the engine bay work:

https://scontent.fper1-1.fna.fbcdn.net/hphotos-xal1/v/t1.0-9/12342375_739749349489817_561763944481051029_n.jpg?oh=a64ba59ff74b3732d136bee3a68e5541&oe=57789250


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xla1/v/t1.0-9/12373322_739749369489815_2148881420821307057_n.jpg?oh=38dd52e4ab175927f6ba44ace179f4d9&oe=57B55618


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xlp1/v/t1.0-9/12310493_739749379489814_7731052508837735902_n.jpg?oh=ae66643dac34f73196e0176a7278994d&oe=5780B10F
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Then started work on the right hand drive dash conversion:

https://scontent.fper1-1.fna.fbcdn.net/hphotos-xla1/v/t1.0-9/12391959_741334899331262_4475278498750866607_n.jpg?oh=e06cb4d3526036fc9b9920669eceface&oe=57BE4552


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xla1/v/t1.0-9/12321538_741334922664593_3643325303806238898_n.jpg?oh=57fe05f790eecb837e36b8b91e0e5b6f&oe=57795F2C


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xfp1/v/t1.0-9/12359844_741334819331270_1716637366578023144_n.jpg?oh=7c5f2826679011450e448552be8f5801&oe=57B8B92C


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xlp1/v/t1.0-9/s851x315/12931254_798945526903532_5260624263917876022_n.jpg?oh=807c6030185e566407e7a8fdaedbd4dd&oe=57B6B9B1


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xtf1/v/t1.0-9/12931136_798945573570194_9131486631082633915_n.jpg?oh=792f22f5eb078574dfb3b1c1140285c8&oe=57BEE0B9


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xfp1/v/l/t1.0-9/12417538_798945586903526_8566567572142829854_n.jpg?oh=5740dc2843e76e5bfc6afb35b55098ee&oe=57768950


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xpf1/v/t1.0-9/12974371_802208306577254_8569944647989937543_n.jpg?oh=e4bb185a28e54d63bb15d8df8c9c1aab&oe=57BB88D3


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xft1/v/t1.0-9/12985453_802208329910585_8973708909978241015_n.jpg?oh=6ce69290580e3df46afc109a767c9059&oe=57BA62EA


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xta1/v/t1.0-9/12439306_802208393243912_5298244705617639228_n.jpg?oh=85758fdf49bbc648ab422bc785ca02ba&oe=57AFCCFC


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xlp1/v/t1.0-9/13007218_802711169860301_3053634085321121057_n.jpg?oh=3199b3b88908b0ba2124c9fa8d9d269f&oe=57B7F0FE


https://scontent.fper1-1.fna.fbcdn.net/hphotos-xlp1/v/t1.0-9/12974311_802711179860300_6556312610332570707_n.jpg?oh=7ac229d0943ca011c2cdd68291710725&oe=57B99F2B
davro
davro
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Very nice work, the Alufibre dash binnacle looks like an interesting layup Smile 



David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
davro (16/04/2016)
Very nice work, the Alufibre dash binnacle looks like an interesting layup Smile 


It's not one I'd recommend Crazy

Alufibre is a nightmare of a material to work with. 
VVS
VVS
Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)
Group: Moderators
Posts: 226, Visits: 334
Great work, thanks for sharing.

its always interesting to see what people are making.




agree with davro, that binnacle looks fun to work.and the dash looks a beast.




what's the yellow stuff you used in the radiator build?
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Extruded polystyrene. I think it's pink really, just the lighting making it look yellow there I think. I normally use polyurethane, but the extruded polystyrene was the perfect thickness for what I needed on that piece. 
VVS
VVS
Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)
Group: Moderators
Posts: 226, Visits: 334
Ok, have you used car body filler over that or a special/ dedicated product.
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yeah regular process, layer of 225g csm over the foam and then body filler from there. 
VVS
VVS
Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)Supreme Being (3K reputation)
Group: Moderators
Posts: 226, Visits: 334
Nice work!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search