I have heard that bondo dont stick to epoxy primer. 

What about epoxy resin? I have a part that I have made with epoxy resin, can I use bondo on it and then paint it?
Hanaldo
Hanaldo
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I've never had any issues. 
Dravis
Dravis
Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)Supreme Being (5.3K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
I keep hearing references to this "Bondo" -- What is that exactly?   Some kind of Polyester filler/primer?

I use cheap polyester filler on a lot of my patterns, I've never had any problems with mixing it with Epoxy .. As long as it is allowed to cure for at least 24 hours .

I often make patterns out of cheap floor insulation foam .. it will "melt" when in contact with the EC pattern primer, so I "seal it" with a layer of epoxy, leave it to cure for 24 hours, key it with 120 grit, then use polyester filler and EC pattern Coat primer -  If I accidentally sand all the way through to the foam, I just re-seal it with epoxy, then carry on with the Pattern Coat primer ..

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Edited 10 Years Ago by Dravis
Hanaldo
Hanaldo
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Bondo is just a brand (the original brand I believe) of polyester body filler. 
f1rob
f1rob
Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
A polyester will stick to an epoxy a lot better than a epoxy will stick to a polyester even thou the epoxy is stronger

Never had any problems but surface prep is important
kidpaint
kidpaint
Supreme Being (800 reputation)Supreme Being (800 reputation)Supreme Being (800 reputation)Supreme Being (800 reputation)Supreme Being (800 reputation)Supreme Being (800 reputation)Supreme Being (800 reputation)Supreme Being (800 reputation)Supreme Being (800 reputation)
Group: Forum Members
Posts: 99, Visits: 676
youll be fine. Ive often had to fix little spots after I have sanded the primer and the guide coat showed the low spot. Make sure the primer is rough sanded so it has a bite for the filler to stick to
Edited 10 Years Ago by kidpaint
67redrocket
67redrocket
Supreme Being (423 reputation)Supreme Being (423 reputation)Supreme Being (423 reputation)Supreme Being (423 reputation)Supreme Being (423 reputation)Supreme Being (423 reputation)Supreme Being (423 reputation)Supreme Being (423 reputation)Supreme Being (423 reputation)
Group: Forum Members
Posts: 49, Visits: 486
Hanaldo (31/03/2016)
Bondo is just a brand (the original brand I believe) of polyester body filler. 


I did not know that, i thought Bondo was another name for body filler. Not always easy to transfer from norwegian Smile

Thank you all for feedback Smile 
Hanaldo
Hanaldo
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
f1rob (31/03/2016)
A polyester will stick to an epoxy a lot better than a epoxy will stick to a polyester even thou the epoxy is stronger

Never had any problems but surface prep is important


Not to hijack the thread too much, but you've brought this up at an interesting time for me Rob. I have been discussing the issue of epoxy/polyester bonds with some friends in the gliding scene, one of whom used to make fibreglass boats for a living. For reasons I can not fathom, he absolutely swears by polyester resin. He considers it the be all and end all of composite resins, and refuses to work with epoxy. 

One of the reasons he gave for polyester being better is that it will bond to epoxy,  but epoxy won't bond to polyester. Something that makes absolutely no sense to me, considering polyester is extremely poor at bonding to anything including itself; whilst epoxy is one of the most widely used adhesives around - because it's bloody good at sticking to things.

Now I tried to do a quick bit of research on this topic, but literally EVERYTHING I come across backs up my belief that epoxy bonds to polyester better than the other way around. So I'd love to hear your thoughts on that? 
f1rob
f1rob
Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)Supreme Being (2.1K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
When I first got into this game 82/83 ish pre preg had only been out (or I should say in use in f1) for a couple of years

there was a split between pre preg (floors,rear flips ect) wet lay epoxy vac (endplates,elements ect) and polyester hand lay glass (brake ducts,bodywork ect)

ALL repairs were polyester and the guys who were there had been with lotus cars/moonraker marine/jcl from early 60,s an that's what I was told

never saw any repairs delam
Hanaldo
Hanaldo
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
If they were with Lotus then I don't believe a word they said, their panels are the worst I've worked on! Laugh

That is interesting though, in all seriousness. Would that not just be for speed of the repair? 