Carbon kevlar v pure carbon


Author
Message
PAUL S
PAUL S
Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)
Group: Forum Members
Posts: 11, Visits: 195
Apart from the pleasing look of pure carbon twill in comparison to carbon kevlar twill of the same weight, why choose carbon instead over the stronger hybrid version? say in a car panel.

Price is comparable so in theory the hybrid offers the better performance? Ferrari used the hybrid extensively in the F40, why is it that supercar builders these days use pure carbon, even when the panel is to be painted?
Reply
ArturK
ArturK
Supreme Being (173 reputation)Supreme Being (173 reputation)Supreme Being (173 reputation)Supreme Being (173 reputation)Supreme Being (173 reputation)Supreme Being (173 reputation)Supreme Being (173 reputation)Supreme Being (173 reputation)Supreme Being (173 reputation)
Group: Forum Members
Posts: 19, Visits: 53
In sport cars impact resistance is guaranteed by aluminium honeycomb, not by carbon fiber or even kevlar.

Carbon fiber sheets and composites .
www.dexcraft.com
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
PAUL S - 9 Years Ago
Hanaldo - 9 Years Ago
PAUL S - 9 Years Ago
scottracing - 9 Years Ago
Hanaldo - 9 Years Ago
scottracing - 9 Years Ago
PAUL S - 9 Years Ago
Hanaldo - 9 Years Ago
Dravis - 9 Years Ago
PAUL S - 9 Years Ago
scottracing - 9 Years Ago
PAUL S - 9 Years Ago
ArturK - 9 Years Ago
Hanaldo - 9 Years Ago
Dravis - 9 Years Ago
scottracing - 9 Years Ago
Boss - 9 Years Ago
Zebra - 9 Years Ago
Hanaldo - 9 Years Ago
Boss - 9 Years Ago
Boss - 9 Years Ago
Boozehawk - 9 Years Ago