Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Adhesive epoxy cf to steel?
Adhesive epoxy cf to steel?
Post Reply
Like
6
Adhesive epoxy cf to steel?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Davidpetty1988
Davidpetty1988
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 26,
Visits: 89
Any idea what adhesive to use on epoxy infused carbon fibre to stainless steel?
Thanks
Dave
Tags
Adhesive
bonding
epoxy
steel
Edited
10 Years Ago by
Davidpetty1988
Reply
Like
6
Reply
Davidpetty1988
Davidpetty1988
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 26,
Visits: 89
Cheers hanaldo
Dave
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Adhesive epoxy cf to steel?
Davidpetty1988
-
10 Years Ago
Use a structural epoxy adhesive like Araldite 2014, or Easy Composites ET500. Alternatively, I'm a...
Hanaldo
-
10 Years Ago
Cheers hanaldo Dave
Davidpetty1988
-
10 Years Ago
I have had great success with EC's Voodoo Glu if you are doing a large amount of work, mixing...
davro
-
10 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search