Hi all
Ive replaced a thin carbon visor bracket from my momo helmet, they are originally held in place with 5 rivets but I cannot use normal pop rivets to replace them.
I'm looking at the different adhesives in stock like the ET515 or VM100 for the application. Which would you recommend for bonding the thin carbon hinge to a plastic and leather substrate?
Thanks
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Can't use the composite specific rivets? I've used them with thin carbon and fibreglass. 
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
good ol' sikaflex or tigerseal might work? 