f1rob
f1rob
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 237,
Visits: 4.8K
If you cant get it from the usual suspects its on evil bay at about £16 a tube
Now why ever would you need anything like that where you work !!! ? Lol
Reply
Like
6
scottracing
scottracing
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
Hi Rob. Thanks for the very kind offer, unfortunately at that time of night I'm putting the little one to bed so won't be able to escape. But I will have a look at that wurth stuff. Would you believe they don't have any structural adhesive at work? Crazy
Reply
Like
6
f1rob
f1rob
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 237,
Visits: 4.8K
You could try wurth replast
Actually designed to repair plastic bumpers but it sticks like the proverbial to a blanket ! Due to the fact its designed for plastics it is always ever so slightly rubbery when its cured
Comes in various speeds,the fast one is 1.5 minutes ! We use it in the pit lane when a part HAS to be repaired and we haven't got time for 490
coming your way up the m4 about 8pm on thur can drop a tube in if you want ?
Reply
Like
6
scottracing
scottracing
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
Thanks for the replies.
I was going to use sikaflex initially, but before I bought something that could be used for other jobs like my usual fave dp490 I would see what's available from ec.
The visor connects to the helmet by two bolts though the composite hinge, they aren't structural so could use virtually anything.
Reply
Like
6
Warren (Staff)
Warren (Staff)
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
If there is any doubt as to the structural integrity of the helmet then we would recommend contacting the manufacturer to be on the safe side.
To determine which adhesive is best depends entirely what the substrate plastic is composed of. Both our
ET515 Rigid 15min Epoxy Adhesive
and
VM100 Black 10min Methacrylate Adhesive
are very good adhesives for a range of plastics. However, some very inert plastics such as polypropylene and HDPE can be very hard to bond to. For an item subject to potential impact, our ET515 would offer a better flexural strength than the VM100 for many applications.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
12
ChrisR
ChrisR
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 363,
Visits: 3K
good ol' sikaflex or tigerseal might work?
Reply
Like
6
Hanaldo
Hanaldo
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Can't use the composite specific rivets? I've used them with thin carbon and fibreglass.
Reply
Like
6
scottracing
scottracing
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
Hi all
Ive replaced a thin carbon visor bracket from my momo helmet, they are originally held in place with 5 rivets but I cannot use normal pop rivets to replace them.
I'm looking at the different adhesives in stock like the ET515 or VM100 for the application. Which would you recommend for bonding the thin carbon hinge to a plastic and leather substrate?
Thanks
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search