Feed & vacum line locations


Author
Message
Imiq Paddle Sports
Imiq Paddle Sports
Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)
Group: Forum Members
Posts: 8, Visits: 63


Fellow Composite Companions

I have the hull of a 7.2m long canoe and was undecided of the locations of the resin feed in lines and the vaccum out lines.

My questions are;
  • for this length would a couple of lines in & out work better?
  • draw the resin from one side to the other rather than nose to tail which is longer?
  • Resin feed from the bottom centre of the hull and draw to each end.
Yours,

Undecided
Reply
Imiq Paddle Sports
Imiq Paddle Sports
Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)
Group: Forum Members
Posts: 8, Visits: 63
Hanaldo

Many thanks for the guidance.

Would i require as many vacuum lines as resin feed lines?

Undecided 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search