Fellow Composite Companions

I have the hull of a 7.2m long canoe and was undecided of the locations of the resin feed in lines and the vaccum out lines.

My questions are;
  • for this length would a couple of lines in & out work better?
  • draw the resin from one side to the other rather than nose to tail which is longer?
  • Resin feed from the bottom centre of the hull and draw to each end.
Yours,

Undecided
By Hanaldo - 2/15/2016 10:15:55 AM

Generally no, I've never had an issue with pulling vacuum through one port.