Hi There,

Im  also a residend in coventry,

I usually give it a couple on min before claming the vac line,

I havent experimented witrh different carbon weights

i have found 2 layers of carbon and sorric  works fine for me



The roof is plenty strong enough with this layup


stuart321
stuart321
Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)
Group: Forum Members
Posts: 37, Visits: 178
Hi,
Just starting out with resin infusion to make parts for my rally car and maybe some friends running similar cars.
I've tried a test piece with 1,2,3 layers of CF, kevlar and soric to get a feel for strength of different combos so ready to get started with some proper parts.

2 questions immediately come to mind if those with more experience could comment
- How soon after clamping the infusion line should you clamp off the vacuum line?  Intuitively it seems leaving it open for 5-10mins will help draw out excess resin which minimises unnecessary weight.  Am I thinking right or are there other considerations?
- How does 200 & 295gsm CF cloth compare for strength?  Its 50% more weight but I'm getting the feeling its not 50% stiffer.

Thanks in advance for any pointers and I'm looking forward to sharing details of my progress & hopefully not asking too many stupid Qs Doze

Stuart
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search