SHD,s owners all come from ACG (now cytec)all the many data sheets they produced over the last 20/25 years had various versions of putting glass toes in at various points to help it de gas, No one ever did it thou as it never made any difference !
Be interesting to see if this does do anything ?
Do you have any dealings with Paul Russell at SHD ?
Only rep I know at a composite firm who has actually been there at the coal face and done the job and knows what they are talking about
All the others are just good salesmen who will show you a fantastic flat sample taken off flat glass sheet
Or very good "theoretical" chemists who will tell you how it "should" work
|