Group: Forum Members
Posts: 6,
Visits: 21
|
I was able to achieve good results by creating vinyl stencils (you can cut them by using any kind of cutting printer like silhouette portrait), applying them on carbon fiber, and then sandblasting the area. I then degrease it and paint it over with any automotive paint, then a layer of clear coat. Remove the vinyl, polish the area, and it will stay forever. You could also use a primer before painting, but in my case it didn't need it. Hope this helps
|