Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
GC100 gelcoat wont get tacky when acetone is allyed
GC100 gelcoat wont get tacky when acetone is allyed
Post Reply
Like
2
GC100 gelcoat wont get tacky when acetone is allyed
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
67redrocket
67redrocket
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 49,
Visits: 486
I did an infusion yesterday and the coat only cured for a hour, but there was no tack after i sprayed it with acetone. I read in another thread that this no longer worked. Why is this not working anymore?
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
GC100 gelcoat wont get tacky when acetone is allyed
67redrocket
-
10 Years Ago
The formulation has been changed to give a longer open time (it can be left longer and still achieve...
Hanaldo
-
10 Years Ago
I have (mistakenly) used acetone to activate some tack after the gel had been left overnight, but...
MarkMK
-
9 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search