By 67redrocket - 12/31/2015 10:20:37 AM
I did an infusion yesterday and the coat only cured for a hour, but there was no tack after i sprayed it with acetone. I read in another thread that this no longer worked. Why is this not working anymore?
|
By MarkMK - 1/1/2016 7:04:52 PM
I have (mistakenly) used acetone to activate some tack after the gel had been left overnight, but this appeared to damage the coating's appearance and leave the surface suffering from pinholes. A decent spray tack will help you out and shouldn't leave any visible markings so long as you don't fo too heavy with it
|
|