Group: Forum Members
Posts: 460,
Visits: 5.2K
|
Don't use spray glue as you will not have a bond between the gel coat and the rest of the layup. Try wiping a bit of acetone on the cured surface then make up some resin and put some on top then continue with your layup.
|