I have read that spray glue is not recomended to use om The mould on cosmeticparts. I coated my mould With The GC50 gelcoat and it cured to much for me so ther was no tack in it to make The carbonfibre stick to The mould. Is it possible to use spray glue instead, when The gelcoat has cured too long?