If you're using EC's epoxy tooling gelcoat, then I've found this to be much more prone to trapping air and leaving behind mini-craters on the surface. It's a fair bit thicker than the Unimould gelcoat and can be tricky to apply well, especially in corners where it might naturally pool a little more
It's also near impossible to carry out good repairs on, as it doesn't respond well to flatting and polishing so I try to avoid using it now on anything but simple shapes.
On balance, I feel the Unimould system is much better to work with, even having the unavoidable fumes to contend with
|